Material number 1.7218     -     25CrMo4

 
Composition in % :

C

Si

Mn

P

S

Cr

Mo

Ni

0,22 - 0,28

max. 0,40

0,60 - 0,90

max. 0,035

max. 0,035

0,90 - 1,20

0,15 - 0,30

 

V

W

Ti

Cu

Al

Nb

B

N

 

 

 

 

 

 

 

 


Range of application and heat treatment :

Heat treatable steel / Cold extrusion steel : crankshafts , axle arm , connecting rods 
Hardening : 840 - 880 °C (oil or water)          Soft annealing : 680 - 720 °C          Normalising : 860 - 900 °C 

General and distinctive features :

 
 

Material selection

Analyses selection

Pictures